Evaluating the Potentials of Liberation Size Determination in Anka (Zamfara State, Nigeria) Manganese Ore and its Communition Tendency using Bond Index Technique
Y. E. Gbadamosi, O. O. Alabi, J. O. Borode
Journal of Materials Science Research and Reviews · pp. 257–268 · Published 16 Jun 2021
Abstract
The present level of exploitation of Manganesemineral from its ore is very low due to depletion of its ore; therefore, there is need for appropriate processing technique that will help in providing solution to the exploitation problem encountered. Chemical, Petrological, Mineralogical, Fractional sieve size analysis and work index of the Anka manganese ore in Anka town of Zamfara state, Nigeria was investigated. 500 g of the ore was weighed using digital weighing balance. The sample was crushed and ground to 80 % passing 250μm sieve size. The ground ore was analyzed using the Energy dispersive X-ray fluorescence spectrometer (ED-XRFS), X-ray Diffractometer (XRD), Scanning electron microscope equipped with dispersion spectrum analyzer (SEM-EDX) and Leica Petrological Microscope. Fractional sieve analysis of the crude sample was carried out at sieve range of 1000-63µm towards particle size distribution and liberation size determination. 500 grams of manganese ore and quartz were sampled and prepared by crushing and grinding to 100% passing 1200μm sieve. 100 grams of prepared ores were charged into array of sieve arranged in √2 series. Set of sieves were mounted on automated Endecott sieve shaker and was operated for 20 minutes. ED-XRFS results shows 77.81% MnO, 10.9% Fe2O3, 4% Al2O3 while the mineralogical analysis reveals Spessartine (3MnO.Al2O3, 0.830), Silicon oxide (SiO2, 1.122), Quartz (SiO4, 0.728), Pyrolusite (MnO, 1.543), and Almandine (Fe3Al2SiO12, 1.583) were identified as the major phases in the ore and the petrological analysis of the crude samples reveals the presence of heavy mineral and segregation distribution of the mineral. The particle size analysis carried out on the Anka Manganese ore revealed that the manganese bearing mineral can be liberated at the particle size fraction of -180 + 125 μm. The work index of the Anka Manganese ore was found to be 14.16 Kwh/ton using the Gaudin Schumann Expression and it falls within the range indicated in literatures as standard which is 10-15.14 Kwh/ton.
Cited by 0
No indexed citations yet.
Related research
- Influence of Compounds Contents and Particle Size on Some Functional Properties of Moringa oleifera Leaves (Lam) Powders — shares topic coverage
- Effect of Distributor Plate Configuration on Pressure Drop in a Bubbling Fluidized Bed Reactor — shares topic coverage
- The Influence of Particle Size and Soaking Time on Surface Hardness of Carburized AISI 1018 Steel — shares topic coverage
- Effects of Sodium Metabisulphite and Blanching Pretreatments on the Quality Characteristics of Yam Bean (Pachyrhizus erosus) Flour — shares topic coverage
- Traditional Production, Processing and Quality Attributes of Ziziphus mauritiana in Savannah Region of Cameroon — shares topic coverage
Article metrics
Real usage data collected on this platform.
0
Page views
0
PDF downloads
0
Outbound clicks
0
Citations
Views by country
Approximate, from request IP at view time — not citizenship or institution. Countries with fewer than 5 views are grouped as "Other".
No views recorded yet.
Traffic sources
Referring site, by host.
No traffic recorded yet.
Views and downloads exclude known bots/crawlers. Citations combines this platform's own DOI-resolved index with each external source's own reported total — see Cited by above for individually listed citing works. Last refreshed 0 seconds ago.