Abstract

Wafer passivation or the protective layer of the internal circuitry of the die plays a major role of providing protection and the isolation of electrical stability of the active circuit on the top area of the wafer. Passivation is normally a screen of an oxide layer on the surface of the silicon wafer or the carrier of internal circuitry of the die. Passivation is normally in the form of polyimide or a glass material. From the wafer structure, it is important to cover the active circuit to ensure no other noises will be induced to the wafer. Inclusion of the passivation layer will help maximize the functionality of the semiconductor device thus eliminating noises coming from the external sources. As the integrated circuit (IC) package goes thinner, the requirement of having the active circuit or the die thinner is the main concern during the wafer preparation process. Wafer backgrinding or wafer thinning is the focal process involved to satisfy such requirement. Prior performing the wafer thinning process, the application of tape, normally in a form of polyolefin or polyvinyl chloride should be performed to eliminate contamination and protects the active layer of the wafer during the process. However, there should be enough adhesion between the wafer and the thinning tape itself. High adhesion strength may lead to adhesive remains or worst, passivation will be peeled off from the active layer of the wafer. Adhesion to the passivation layer should be properly evaluated and monitored in such way that will eliminate adhesive remains during detaping process after wafer thinning. The effect of adhesion strength could be predicted by properly selecting thinning or protective tape to be used. Higher adhesion strength could be achieved but due to criticality of passivation to tape adhesion, ultra-violet (UV) process should be included to substantially decreased the adhesion. The importance of UV exposure is also discussed on this paper.

Wafer tape wafer preparation pre-assembly ultraviolet passivation adhesion.

Cited by 2

Minimizing floating defects in wafer taping through visual recognition and response surface optimization

Cheng-Tang Pan, Po-Chun Lee, Pin-Zheng Wang · Journal of Engineering Research · 2026

Laser DAF Cut Augmentation for Thin Wafers

B. C. Bacquian, F. R. Gomez · 2020

Article metrics

Real usage data collected on this platform.

0

Page views

0

PDF downloads

0

Outbound clicks

2

Citations

Views by country

Approximate, from request IP at view time — not citizenship or institution. Countries with fewer than 5 views are grouped as "Other".

No views recorded yet.

Traffic sources

Referring site, by host.

No traffic recorded yet.

Views and downloads exclude known bots/crawlers. Citations combines this platform's own DOI-resolved index with each external source's own reported total — see Cited by above for individually listed citing works. Last refreshed 0 seconds ago.