Abstract
Fe-Co-2V is a popular metallic alloy used in electromagnetic applications. However, there is a lack of mechanical fatigue characterization of this alloy in the literature. In this work, Fe-Co-2V specimens with rectangular cross-sections were carefully prepared in accordance with standards. They were measured for surface roughness and then subjected to quasi-static monotonic testing, as well as fatigue testing at both 0.5 Hz and 1 Hz frequencies. Both Rockwell hardness and Vickers micro-hardness testing were performed. Additionally, scanning electron microscopy imaging of the fractured surfaces was done. The quasi-static testing revealed a flat yield region characteristic of Lüders bands. The fatigue results did not show significant differences or sensitivity to change in frequency, although the fatigue life was higher on average for the 0.5 Hz. However, the fatigue results differed from published work at 0.33 Hz. The fractography revealed purely brittle fracture, with clear chevron marks and fracture initiation always starting at the surface. Lastly, it was identified that the C, D, and F Rockwell hardness scales were appropriate for testing this material and that the grain size necessitated the use of the upper end of indentation force for Vickers micro-hardness testing.
Cited by 0
No indexed citations yet.
Related research
- The Association between Depression, Daytime Sleepiness, Chronotype and Fatigue among the Students — shares topic coverage
- Material Selection for Gas Turbine Blade Coating Using GRANTA Material Selector — shares topic coverage
- A Three Dimensional Finite Element Analysis for Contact Stress and Fatigue near the Fir-Tree Region in a Gas Turbine Blade — shares topic coverage
- Modeling the Homeostatic ‘Process S’ to Assess Sleep Misalignment and Excessive Sleepiness in Shift-Workers — shares topic coverage
- A Study on Affordable Homestead Implements for Stress Reduction on Body Parts amongst Farm Workers of Khammam District, India — shares topic coverage
Article metrics
Real usage data collected on this platform.
46
Page views
0
PDF downloads
5
Outbound clicks
0
Citations
Views over time
Views by country
Approximate, from request IP at view time — not citizenship or institution. Countries with fewer than 5 views are grouped as "Other".
Traffic sources
Referring site, by host.
Views and downloads exclude known bots/crawlers. Citations combines this platform's own DOI-resolved index with each external source's own reported total — see Cited by above for individually listed citing works. Last refreshed 0 seconds ago.