Research Article Open access CC BY 4.0

Mechanical Characterization of Fe-Co-2V (Hiperco): Fatigue/Monotonic Testing, Hardness Testing and Fractography

Elisabeth Keller, Tariq A. Khraishi, Kyle Johnson

Journal of Materials Science Research and Reviews · pp. 253–270 · Published 19 Sep 2020

Abstract

Fe-Co-2V is a popular metallic alloy used in electromagnetic applications. However, there is a lack of mechanical fatigue characterization of this alloy in the literature. In this work, Fe-Co-2V specimens with rectangular cross-sections were carefully prepared in accordance with standards. They were measured for surface roughness and then subjected to quasi-static monotonic testing, as well as fatigue testing at both 0.5 Hz and 1 Hz frequencies. Both Rockwell hardness and Vickers micro-hardness testing were performed. Additionally, scanning electron microscopy imaging of the fractured surfaces was done. The quasi-static testing revealed a flat yield region characteristic of Lüders bands. The fatigue results did not show significant differences or sensitivity to change in frequency, although the fatigue life was higher on average for the 0.5 Hz. However, the fatigue results differed from published work at 0.33 Hz. The fractography revealed purely brittle fracture, with clear chevron marks and fracture initiation always starting at the surface. Lastly, it was identified that the C, D, and F Rockwell hardness scales were appropriate for testing this material and that the grain size necessitated the use of the upper end of indentation force for Vickers micro-hardness testing. 

Hiperco fatigue quasi-static Lüders bands Vickers Rockwell surface roughness.

Cited by 0

No indexed citations yet.

Article metrics

Real usage data collected on this platform.

46

Page views

0

PDF downloads

5

Outbound clicks

0

Citations

Views over time

Views by country

Approximate, from request IP at view time — not citizenship or institution. Countries with fewer than 5 views are grouped as "Other".

Traffic sources

Referring site, by host.

Views and downloads exclude known bots/crawlers. Citations combines this platform's own DOI-resolved index with each external source's own reported total — see Cited by above for individually listed citing works. Last refreshed 0 seconds ago.